Sample - eSun ePLA-LW (Light Weight)
Printing speed
40-80mm/s
Note: Printing test conditions: nozzle 190-280℃; layer height 0.2mm; bed 45℃; speed 40mm/s
1. Note that the first layer speed setting is consistent with the actual printing speed, set to 100% of the actual printing speed, turn off the first layer and small area printing speed reduction function, the first layer extrusion rate is consistent with the actual foaming extrusion rate, such as 270 degrees set to 45% of the first layer extrusion rate; if the bed adhesion is too strong, you can set the bottom valve when printing.
2. Pay attention to the maximum operating temperature of the printer. Most Teflon tube printers cannot be operated for a long time above 250℃. Long-term printing above this temperature may cause blocking. If the temperature exceeds 250℃, high temperature printers such as metal hoses are required for printing.
3. Yellowing of printed parts after high temperature foaming is a normal phenomenon. Lowering the printing temperature can relieve it.
4. Since the ePLA-LW foams continuously in the melting cavity of the high-temperature nozzle, the retraction basically does not work. Stringing is normal during printing. It is recommended to print the rc plane in vase mode to reduce the effect of stringing.
5. Foaming ratio is related to temperature, printing speed, nozzle melting cavity size, pay attention to compare model design wall thickness according to your own printing situation, adjust extrusion rate, temperature, speed and other parameters.
DISCLAIMER: BITS4BOTS LIMITED nor any of its Subsidiaries has any material liability (whether known or unknown, whether asserted or unasserted, whether absolute or contingent, whether accrued or unaccrued, whether liquidated or unliquidated, and whether due or to become due) arising out of any injury to individuals or property as a result of the ownership, possession or use of any product manufactured, sold, leased or delivered by BITS4BOTS LIMITED or any of its Subsidiaries.